Place of Origin: | Anping Hebei Province |
---|---|
Brand Name: | Yuanqiao |
Certification: | TUV Reach SVHC233 |
Model Number: | YuanQiao-123 |
Minimum Order Quantity: | 1 Roll |
Price: | 0,6USD /Pic |
Packaging Details: | Wooden boxes or pallet or as required |
Delivery Time: | Within 7 days |
Payment Terms: | T/T |
Supply Ability: | 1000 pcs per day |
Product Name: | Copper Mesh | Key Words: | Knitted Copper Mesh |
---|---|---|---|
Length: | 10M | Weaving Type: | Knitted |
Processing Service: | Cutting | Width: | 127mm |
Application: | Weeping Hole | Color: | Natural Copper |
High Light: | Copper Knitted Mesh Customized,Copper Knitted Mesh 10M Length,Customized Knitted Copper Mesh |
Knitted copper wire mesh has the same structure as stockings or sweaters. The copper gauze is made of pure copper wire knit into a continuous flat double-thick stocking. 100% copper material is never rust during its long lifespan.Knitted copper mesh is widely used in industrial industry and used as rodent exclusion mesh.
Product Name | Copper Knitted Wire Mesh | Key Words | Knitted Wire Mesh |
---|---|---|---|
Material: | 99.9% Copper Wire | Wire Type: | Round Wire, Flat Wire |
Mesh Width: | 4in, 5in, 6in, As Per Order | Other Name: | Copper Gauze |
Mesh Status: | Plain, Or Crimped | Strand Number: | 1, 2 Or 4. |
Copper mesh for weeping hole,because of the copper color the same as roof ,so after fill into the mesh ,you will like it very much
Steps to clean the screws and barrels efficiently with copper gauze and grease.
Step 1: Use a purging compound to clean the extruder. Then use small ball of copper mesh with some silicone grease on it to clean the die face. Also please clean the valve when it is still hot.
Step 2: Remove the die from the extruder head. It is best to clean it by silicone coated copper gauze forced through the die with a wooden dowel.
Step 3: Pull back and forth the copper gauze to complete the cleaning after it pass through the die.
Step 4: Make sure that no residual trace of adhered plastic is left, nor causing a scratch on the metal surface, so the die is thoroughly clean.
Step 5: Remove the hot screw partly, wrap the copper gauze with silicone coating 3 times around the screw, pull back and forth to do the cleaning.
Step 6: Keep sliding the copper gauze when removing the screw out of barrel slowly, until the screw is clean. It takes only 5 minutes for step 5 and 6 operations.
Step 7: Wrap copper mesh at end of a long rod and pass it through the barrel. Then, chuck the rod into power drill, insert fresh gauze and pass back and forth through barrel until clean.
Step 8: Please do all the operations with silicone grease coated copper mesh. Now all parts is clean and ready for reassemble.
Useful shielding to suppress electromagnetic signals passing through flashing windows
Copper has good electrical conductivity, thermal conductivity, corrosion resistance and ductility and other physical and chemical properties.Electrical and thermal conductivity is second only to silver, pure copper can be drawn into very fine copper wire, made into very thin copper foil.The fresh cross section of pure copper is rose-red, but after the formation of copper oxide film on the surface, the appearance is purplish red, so it is often called copper.